Homogenization of a slowly cooled cu-ni alloy having a


1. What is spray atomization?

2. Homogenization of a slowly cooled Cu-Ni alloy having a secondary dendrite arm spacing (SDAS) of 0.025 cm requires 8 hours at 1000°C. Design a process to produce a homogeneous structure in a more rapidly cooled Cu-Ni alloy having a SDAS of 0.005 cm

Request for Solution File

Ask an Expert for Answer!!
Mechanical Engineering: Homogenization of a slowly cooled cu-ni alloy having a
Reference No:- TGS01677810

Expected delivery within 24 Hours