An fcc iron-carbon alloy initially containing .2 wt% carbon is carburized at an elevated temperature and in an atmosphere where in the surface carbon concentration is maintained at 1.0 wt%. If after 49.5 hrs, the concentration of carbon is .35 wt% at a position 4 mm below the surface, determine the temperature at which the temperature was carried out.