Determine the carburizing time necessary to achieve a carbon concentration of 0.35 wt% at a position 2 mm into an iron-carbon alloy that initially contains 0.10 wt% C. The surface concentration is to be maintained at 1.30 wt% C, and the treatment is to be conducted at 1000oC.