Determine the carburizing time necessary to achieve a carbonconcentration of 0.45 wt% at a position 2 mm into an iron-carbonalloy that initially contains 0.20 wt% C. The surface concentrationis to be maintained at 1.30 wt% C, and the treatment is to be conducted at 1000oC.