An FCC iron-carbon alloy initially containing .20wt% C is carburized at an elevated temperature and in an atmosphere wherein the surface carbon concentration is maintained at 1.0wt%. If after 49.5 h the concentration of carbon s .35wt% at a position 4.0mm below the surface, determine the temperature at which the treatment was carried out.