The lower yield point for an iron that has an average grain diameter of 5 x10-2 mm is 135 MPa (19,500 psi). At a grain diameter of 8 x 10-3 mm, the yield point increases to 260 MPa (37,500 psi). At what grain diameter will the lower yield point be 205 MPa (30,000 psi)?