A window is etched through a 500 nm thick oxide on a 100


A window is etched through a 500 nm thick oxide on a [100] silicon wafer. The wafer is re-oxidized at 1100 °C using wet oxidation to grow a 750 nm thick film inside the window. Draw a cross-section of the wafer following the second oxidation. Give numerical values for the step heights at the interface and at the surface of the oxide.

Request for Solution File

Ask an Expert for Answer!!
Electrical Engineering: A window is etched through a 500 nm thick oxide on a 100
Reference No:- TGS0589584